Plastic bending creep testing machine

NegotiableUpdate on 05/12
Model
Nature of the Manufacturer
Producers
Product Category
Place of Origin

Overview

参考- ASTM E139-96 Standard Test Methods for Conducting Creep, Creep-Rupture and Stress-Rupture test of Metallic Materials

Product Details

DESCRIPTION

This product adopts the method of direct load loading on the sample. Generate tensile and bending deformation phenomena in plastic material samples, and use displacement sensors to deform the samples according to the required form for detection. Use a high-temperature chamber to control the temperature of the sample at 20-200 ℃, with a temperature sensor and controller placed in each chamber. The length of the tensile test specimen is 25mm as the standard specimen. The bending test maintains the span distance of the specimen at 50mm.

refer to

- ASTM E139-96 Standard Test Methods for Conducting Creep, Creep-Rupture and Stress-Rupture test of Metallic Materials

- ISO 204 Metallic materials- Uniaxial creep testing in tension-Method of test

Product specifications

host

The part that directly applies load to the sample

• Frame material: Square structural steel pipe STKM400

• Load consumption: 300kg/ch,

Load precision: ± 1%

• Use cylinder load loading method or use weights to directly load the load method

Installation methods for regulators, air solenoid valves, proportional control valves, and weighing sensor cylinders

Horizontal caster installation - height adjustable caster

Stretching and bending fixtures

• Stretch fixture

- Capacity: 500kg

-Specimen thickness: Max within 8mm

- Type: Wedge action grip

- Jaw face rough machining

-Even with thinner specimens used for testing, it can sustain constant load loading

• 3-point bending fixture

-Span distance: 50mm

-Roll diameter: 10mm

-Roll surface coating treatment

-Sample Installation Guide

-The support point did not shake during the experiment

-Prevent impact collision between equipment and accessories

-Prevent deformation of accessories and measurement errors caused by temperature changes

Strain sensor

• Digital displacement sensor (bending)

- Stroke: 25㎜

-Resolution: 1 μ m

-Form: Digital Linear Table - No Calibration Required

-The battery can be used continuously for 7000 hours

-Pull rod material: STS 303, 17-18 (10-6/℃)

-External installation of high and low temperature box

High temperature box and temperature control device

High temperature test environment control device

• Temperature: 20~200 ℃, maximum 250 ℃, minimum 15℃

• Use ink cartridge heater

Internal dimensions: 250mmW x 250mmD x 250mmH x 4chamber

Two samples can be placed in one test chamber

Single phase, 220V, 50/60Hz, maximum, 5kW

Thermostat installation

• Temperature difference: ± 1 ℃ temperature difference between each sample

The overall interior of the high-temperature box: ± 2 ℃

Internal material: Polished STS 304

• External material: SS400&heat-treated coating

Noise standard below 50dB

Front internal observation window

Installation of internal LED lights

Installation of ink cartridge heaters with a capacity of 600W x 2set or higher

• 와류 발생 팬 장착

Thermocouples: K-type, 2/high temperature box

Thermocouple error: within ± 1.0 ℃ or ± 0.4% of the measured temperature

•KOLAS regulations stipulate that documents should be attached and pasted on Thermocouples and controllers

• Filling insulation materials (ceramic insulation block filling reinforcement)

Install a cooling radiator for each high-temperature chamber

Installation of refrigeration unit for cooling

-Water tank capacity: 45 liters

-Circulating pump: 300W

-Temperature range&Cooling: 5 ℃~30 ℃

-Power supply: AC 3-phase, 220V, 380V, 440V, 4.6kW

-Abnormal and safety devices: Low water, EOCR motor protectors (water pump, COMP, fan), low pressure cut-off, high pressure cut-off, high temperature box and temperature control device

temperature controller

• Digital temperature controller

For easy control of high and low temperature boxes (1), temperature confirmation (1), each high and low temperature box is equipped with two thermocouples and temperature controllers

Installation of temperature control rack

Refrigerator on/off, heater on/off, power switch

• Control connectors&wiring

50ms high-speed acquisition and ± 0.3% high-precision display

Heating and cooling control function simultaneously

• Computer communication support: RS 485

• Large screen display and high brightness LED for easier operation and viewing

• Heater disconnection alarm function

• Output control: Relay electric shock output

SSR output

current output

Control mode: On/Off, P/PI/PD/PID control

• Power supply: Voltage rating at 100 to 240 VAC (±10%), 50/60 Hz

• Temperature controller rack

• Alarm lamp

Creep testing machine controller

function

-Computer and SD card data storage: time, displacement, temperature of each channel

-Temperature controller and communication function (using a computer to set and control temperature)

-Automatic power-off function of high and low temperature chambers after the experiment is completed

-Test restart function corresponding to instantaneous power outage (computer with UPS installed, UPS provided by the user)

-Condition setting and emergency stop function

-Emergency stop button, high and low temperature box on/off button, LED on/off button

- National instrument

- DAQ : 100Hz

- A/D channel: 3

- Analog output: 2

- DIO Input/Output: 4

- Sensor data log output: 2

- Control type: PCI

Software and data acquisition system

function

• Data collection and storage - temperature, displacement, time, strain, inclination

Time and strain status display function for each channel (real-time/selected time, can be changed according to user requirements before delivery)

• Test information and test condition input (can be changed according to user requirements before delivery)

Time units (hr, min, sec), displacement (strain,%, mm), and basic settings can be made during the test setup

• Compatibility with Excel programs

• Temperature display

• Basic information input function at the beginning of the experiment

• Use programs to control devices

• Temperature correction function (can be changed according to user requirements before delivery)

Individual opening/closing of each channel (can be changed according to user requirements before delivery)

• Display of test time and end time

Time process setting function - preheating function setting

Start time setting

Test stop function when the end condition is met

• Data storage format setting function - data saving speed setting function (6 or more are one unit)

Displacement change element storage function

Time variation storage function

Process change data storage function

• Safety function settings - time, load, temperature

• Chart display function - time: displacement, time: strain

• Display function - test time, current temperature and average temperature, displacement, strain